Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 47.6 MPa | 6910 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |