Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 475 MPa @Strain 0.200 % |
68900 psi @Strain 0.200 % |
|
Haynes 188 alloy, plate at RT after 4000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 475 MPa @Strain 0.200 % |
68900 psi @Strain 0.200 % |
|
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 475 MPa @Strain 0.200 % |
68900 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature sheet after 100 hours of 760°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 475 MPa | 68900 psi | |
Haynes Hastelloy® alloy 625 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |