Polymer Property : Tensile Strength, Yield = 68200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 470 MPa

@Strain 0.200 %
68200 psi

@Strain 0.200 %
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 470 MPa

@Strain 0.200 %
68200 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature after 25% cold reduction, 1175°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 470 MPa

@Strain 0.200 %
68200 psi

@Strain 0.200 %
Haynes 625 alloy, plate after 1000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Yield 470 MPa
68200 psi
Haynes Hastelloy® alloy 718 12.7 mm plate weldments
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield >= 470 MPa

@Strain 0.200 %
>= 68200 psi

@Strain 0.200 %
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Rolled Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin..
Tensile Strength, Yield 470 MPa

@Strain 0.200 %
68200 psi

@Strain 0.200 %
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 8.5% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..
Tensile Strength, Yield 470 MPa
68200 psi
0.2% offset; ASTM E8
3D Systems LaserForm™ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing
Parts fabricated from this rapid prototype metal material are actually a blend of stainless steel and bronze. The part is built with steel and subsequently infiltrated with bronze. A6 is great for ..
Tensile Strength, Yield 470 MPa
68200 psi
EN2597B
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/7581
Fiber: E-Glass, Weave: 8HS, 300 g/m2Information provided by HexCel
Tensile Strength, Yield 470 MPa

@Strain 0.200 %
68200 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature after 0% cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall..