Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 46.1 MPa | 6690 psi | ASTM D412 |
C.O.I.M. LARIPUR® LPR9060 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |