Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 45.5 MPa | 6600 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L0248 Opaque Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L0248 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
PolyOne Nymax™ 2024 HS UV 425C Grey Polyamide 66 (Nylon 66) The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o.. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | Type I bar at chs 2 in per min; ASTM D638 |
Network Polymers NPP 908 Description: Polyester CopolymerInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | 2 in per min; ASTM D638 |
Network Polymers SBN 150 Styrene Butadiene Acrylonitrile Terpolymer Description: Styrene Butadiene Acrylonitrile TerpolymerInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Polymer Resources ABS-G5 ABS, 5% Glass Reinforced Acrylonitrile Butadiene Styrene, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Polymer Resources ABS-G5-[color]-3 ABS, 5% Glass Reinforced, UV-stabilized Acrylonitrile Butadiene Styrene, 5% Glass Reinforced, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings 87322 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 45.5 - 108 MPa | 6600 - 15600 psi | Average value: 74.5 MPa Grade Count:40 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Tensile Strength, Yield | 45.5 - 66.0 MPa | 6600 - 9570 psi | Average value: 57.9 MPa Grade Count:59 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PCT2018 PC/PBT Alloy PC/PBT alloy with excellent low temperature impact strengthAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Spartech SP-3010 Rigid PVC Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Techmer ES HiFill® PA6 0232 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Westlake Plastics Pomalux® SD-A Acetal Copolymer (anti-static) Non-carbon-filled, permanently static-dissipative material which is non-migratory and non-humidity dependent. With enhanced lubricity, POMALUX SD-A provides superior wear resistance and ease of mac.. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Chevron Phillips MC3700 High Flow Crystal Polystyrene DescriptionChevron polystyrene resin MC3700 crystal is a free-flowing, crystal clear polystyrene injection molding compound, designed specifically for thin- and medium-walled or long-flow, difficult.. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Ensinger Tecaform™ SD Acetal (POM) Ensinger-Hyde static dissipative acetal contains no carbon fibers or powders and is generally accepted for clean room use. With its surface resistivity of 109 to 1011 ohm/square and its excellent b.. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA TW-20 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ASAPC 6141 UV Stabilized Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D-638 |
Axiall 7020 Rigid PVC, Extrusion Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF.. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D-638 |
Axiall 8240 Rigid PVC, Extrusion Georgia Gulf 8240 is a general-purpose rigid PVC extrusion compound designed for applications requiring the following properties: Rigidity/StiffnessGlossImpact Strength & ToughnessFlame RetardantCh.. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Aaron Industries AAROLENE® AVPS GPPS 100-1 Clear, Virgin Polystyrene Resin A general purpose polystyrene resin, specifically designed for all injection molding applications. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | ASTM D638 |
Techmer ES Plastiblend® APC100 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 45.5 MPa | 6600 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-NY-060-CU Polyamide 6 (Nylon 6) Information provided by PolyOne |