Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East) CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli.. |
|||
Tensile Strength, Yield | 45.0 - 60.0 MPa | 6530 - 8700 psi | Compression; ISO 527 |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | |
Ineos ABS Lustran® QE 1120, Extrusion Grade
(discontinued **) General purpose extrusion grade.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with .. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | |
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend
(discontinued **) Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527-1/-2 |
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developed for automotive bezel application that requires basecoat + .. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX1005X PPE+HIPS (Europe-Africa-Middle East) Noryl PX1005X is an unfilled, low heat resistance, halogen free (according VDE/DIN 472 part 813) flame retardant material. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX2245 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2245 is a halogen free (according to VDE/DIN 472 part815) flame retardant material. The material fulfills the IEC 65 part 20.2 requirement at 1.6 mm thickness. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific) PA6 based unfilled GTX. High impact. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ASTM D638 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ASTM D638 |
Eastman Tritan WX500 Copolyester Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | |
Covestro Bayblend® T 45 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BS/2 PA6 Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 16 LM PA12 Product Description: Grilamid L 16 LM is a , low viscosity extrusion type, based on Polyamide 12 (PA12). Grilamid L 16 LM is UV- and heat stabilized. The modification with a nucleation agent results.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 HL black 9563 PA12 Product Description: Grilamid L 20 HL black 9563 is a, medium viscosity extrusion grade, based on Polyamide 12 (PA12). Grilamid L20 HL black 9563 has been especially developed for external cable she.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 LM PA12 Product Description: Grilamid L 20 LM is a medium viscosity Polyamide 12 (PA12) extrusion grade. Grilamid L 20 LM is UV and heat stabilized and has been modified with a nucleation agent which result.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS LC1201 BK040A Nylon 1010
(Unverified Data**) Toughened Renewably Sourced Medium Viscosity Polyamide 1010 Developed for Extrusion Zytel RS LC1201 BK040A is a renewably sourced polyamide 1010 resin containing a minimum of 85% renewably sourced i.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GB6 POM 30% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527 |
Ascend Performance Materials Vydyne® 47 Nylon 66, Conditioned Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MHLS Polyamide 6 - Colored Heat and UV light stabilized grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main proper.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Tensile Strength, Yield | 45.0 - 60.0 MPa @Thickness 2.00 mm, Temperature 23.0 °C |
6530 - 8700 psi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® B3S BK00464 PA6 (Conditioned) Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50mm/min; ISO 527 |
BASF Ultramid® B3S HP PA6 (Conditioned) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |