Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.5 MPa
6450 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging VB7 White 215 Polyvinyl Chloride, Rigid (PVC, Rigid)
A rigid PVC Compound designed for extrusion blow molding balusters for railings.Information provided by PolyOne
Tensile Strength, Yield 44.5 MPa
6450 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Strength, Yield 44.5 MPa
6450 psi
106% Ret.
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 44.5 MPa
6450 psi
106% Ret.
UBE UBESTA® 3030U Nylon 12 (After Hexane for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 44.5 MPa
6450 psi
ASTM D638
Albis Plastics Cellulose Acetate Butyrate B9424-3 , 3% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Copyright © lookpolymers.com All Rights Reserved