Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® HMG47MD ABS General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47N ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 4.0 mm thick, 10.0 mm wide molded rod; ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 7300 PRE-ELEC ESD 7300 is a static dissipative thermoplastic compound based on PC/PBT. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7300 has been developed for inj.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D638M |
DSM Somos® 7120 Epoxy Photopolymer, Green Parts
(discontinued **) DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO R527 |
Fainplast Compounds RE 412/L Rigid PVC, Extrusion Corrugated plastics |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO R527 |
Fainplast Compounds RE 520/1 Rigid PVC, Extrusion Electric pipes |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO R527 |
Fainplast Compounds RE 625 Rigid PVC, Extrusion Spiral pipes |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO R527 |
Fainplast Compounds RL 710 Rigid PVC, Extrusion Corrugated electric pipes |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D638 |
LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp IP003 PA6.12 LNP* Lubricomp* IP003 is a Nylon 6/12 base resin containing PTFE and Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DEF13 PC LNP* Stat-kon* DEF13 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO 527 |
Styrolution Novodur® 650 ABS Novodur 650 is an injection molding grade of ABS with high impact strength, high flow and high gloss.Information provided by Styrolution |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 2 in/min; ASTM Test |
Styrolution Terblend® N NMX04 ABS/PA6 (Dry) Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Europe-Africa-Middle East) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL EXT115 PPE+PS (Asia Pacific) PPE+PS, Auto exterior grade, wax remover resistant |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | dry; ISO 527 |
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.Application: For all kinds of injection molding thin-walled parts.Information provided by Ter Hell Plastic GMBH. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D638 |
Eastman Eastar DN011 Copolyester Eastar Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN011 contains a mold release.Applications/.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D638 |
Eastman Tritan EX401 Copolyester Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D 638 |
Cossa Polimeri ESTADIENE 1640 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D638 |
Eastman Tritan MX810 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D638 |
Eastman Tritan MX811 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceGood heat resistanceO.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Wet; ASTM D638 |
Asahi Kasei Leona® 9400S Nylon 66 Excellent impact resistance. Suitable for thick-wall parts.Applications:Railroad tie insulatorsInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 50 mm/min |
Polimeri Europa SINKRAL PD F332 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MGN,105-15-16-20 General purpose injection grade which combines excellent thermal stability during processing with.. |