Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.7 MPa | 6340 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging VE0-112 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.7 MPa | 6340 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87160 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |