Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 42.5 MPa | 6160 psi | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Tensile Strength, Yield | 42.5 MPa @Temperature 115 - 145 °C, Time 1.80e+7 sec |
6160 psi @Temperature 239 - 293 °F, Time 5000 hour |
5 [mm/min], 50% Loss of Tensile Strength; ICE 216 |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Strength, Yield | 42.5 MPa @Temperature 100 - 120 °C, Time 7.20e+7 sec |
6160 psi @Temperature 212 - 248 °F, Time 20000 hour |
5 [mm/min], 50% Loss of Tensile Strength; ICE 216 |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Strength, Yield | 42.5 MPa @Temperature 100 - 140 °C, Time 1.80e+7 sec |
6160 psi @Temperature 212 - 284 °F, Time 5000 hour |
5 [mm/min], 50% Loss of Tensile Strength; ICE 216 |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Strength, Yield | 42.5 MPa @Temperature 90.0 - 120 °C, Time 7.20e+7 sec |
6160 psi @Temperature 194 - 248 °F, Time 20000 hour |
5 [mm/min], 50% Loss of Tensile Strength; ICE 216 |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |