Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.21 MPa | 610 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase SILASTIC® 7-4860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Yield | 4.21 MPa | 610 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 0470 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 4.21 MPa | 610 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 629 Perfluoroelastomer Chemraz® 629 perfluoroelastomer is specifically developed by Greene Tweed to meet the rigorous demands of aggressive plasma systems. This product’s unique formulation provides enhanced plas.. |
|||
Tensile Strength, Yield | 4.21 MPa | 610 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-265 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 4.21 MPa | 610 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-560 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 4.21 MPa @Strain 300 % |
610 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3780 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |