Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.14 MPa | 600 psi | |
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | ASTM D412 |
Precision Polymer Engineering S50E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 45-55 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci.. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | ASTM D412 |
Precision Polymer Engineering S60E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 55-65 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci.. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | chs 20 in/min; ASTM D638 |
Network Polymers Softflex® 4500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | ASTM D412 |
Polymax® Maxelast® P1955 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 4.14 - 57.0 MPa | 600 - 8270 psi | Average value: 19.9 MPa Grade Count:13 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 655 Perfluoroelastomer Chemraz® 655 is Greene Tweed’s high-temperature off-white perfluoroelastomer. Specifically developed for wafer processes with operating temperatures up to 315°C (600°F), Chemraz 655 p.. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | @50% Elongation; ASTM D1414 |
Greene Tweed Fluoroelastomer 742 FKM Fluoroelastomer 742 performs well in aggressive chemicals and where ultrapure materials are not required. Recommended for conventional wet and dry system applications, Fluoroelastomer 742 has a goo.. |
|||
Tensile Strength, Yield | 4.14 MPa @Strain 300 % |
600 psi @Strain 300 % |
ASTM D412 |
Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma.. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-265 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | >= 4.14 MPa | >= 600 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5488 Nitrile Rubber Low temperature service Nitrile; plasticizer freeInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | at 100%; ASTM D412 |
Lubrizol Estane® ALR E80A Thermoplastic Polyurethane Type: Estane® ALR E80A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Information Provided by The Lubrizol Corporation |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | at 100%; ASTM D412 |
Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 75AT3 is a 75A aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and.. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | 100% Secant; ASTM D638 |
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer AFFINITY™ EG 8200G Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. It exhibits high flexibility and elasticity. It can be utilized in monolayer cast film and in .. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | cured 72 hrs @ RT |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Tensile Strength, Yield | 4.14 MPa @Strain 300 % |
600 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 38-034M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDiscla.. |
|||
Tensile Strength, Yield | 4.14 MPa @Strain 300 % |
600 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT38-034 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDi.. |
|||
Tensile Strength, Yield | 4.14 MPa @Strain 300 % |
600 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3965 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Tensile Strength, Yield | 4.14 MPa @Strain 300 % |
600 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 454 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerApplications:General PurposeCove BaseInteriorMarket:AutomotiveConsumer GoodsBuilding and ConstructionProcessing Method:Extrusion and Molding.. |
|||
Tensile Strength, Yield | 4.14 MPa | 600 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3640 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingInformation provided by PolyOne.. |