Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 41.0 MPa | 5950 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® INP576 ABS Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Tensile Strength, Yield | 41.0 MPa @Temperature 100 °C |
5950 psi @Temperature 212 °F |
ISO 527 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | ASTM D638 |
Ineos Nova 2580 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistanceApplications: Cutlery, Consumer electronicsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optic.. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KA000M POM (Europe-Africa-Middle East) LNP* LUBRICOMP* KA000M is a compound based on Acetal Copolymer resin containg Aramide and Proprietary Lubricant. Added features include Internally Lubricated. |
|||
Tensile Strength, Yield | 41.0 MPa @Temperature 23.0 °C |
5950 psi @Temperature 73.4 °F |
50mm/min; ISO 527-2/1A/50 |
SYNTHOS Forsan® 573 Acrylonitrile Butadiene Styrene (ABS) Increased heat resistant, glossy, good mechanical properties, suitable for electroplating.Applications: Electrotechnics, automotiveHousehold appliances, electric switches, car interior parts, profil.. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East) LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | ISO 527 |
Styrolution Novodur® 970 ABS Novodur 970 is an injection molding grade of ABS with high impact strength and good paintability.Information provided by Styrolution |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP NX07354P PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating performance, a good candidate for Laser Direct Structuring applications. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon AD000Z ABS LNP* Stat-Kon AD000Z is a compound based on ABS resin with carbon powder. Grade characteristics: a statically conductive extrusion grade.This data was supplied by SABIC-IP for the Americas region... |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBF 3779 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | ASTM D638 |
UBE UBESTA® 3020X8 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1605 Glass Reinforced Chemically Coupled Copolymer DescriptionPolyfort® FPP 1605 is a 10% glass reinforced chemically coupled copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | ISO 527 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Tensile Strength, Yield | 41.0 MPa @Strain 300 % |
5950 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 8529 Polyurethane + ABS injection molding grademodified with ABSgood low-temperature flexibilitygood wear resistanceApplicationSki boot shellsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | 50 mm/min; ISO 527 |
Chi Mei Polylac® PA-756S ABS - High Flow Super high flow, medium impact |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | 50 mm/min; ISO 527 |
Chi Mei Polylac® PA-763 ABS - Flame Retardant F.R. High Heat Weather Resistant |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | 50 mm/min; ISO 527 |
Chi Mei Polyrex® PG-33 Polystyrene Standard grade |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436G20CL Glass Reinforced |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | ASTM D638 |
Ashley Polymers Ashlene® 827LD Nylon 6 A very high impact nylon resin for injection molding applications. Outstanding low temperature properties.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | |
Poco Graphite TM Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | 2.0 in/min; ASTM D638 |
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties.. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |
|||
Tensile Strength, Yield | 41.0 MPa | 5950 psi | ASTM D638 |
BP Amoco Amoco® 7635 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR .. |