Polymer Property : Tensile Strength, Yield = 59200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 408 MPa

@Strain 0.200 %
59200 psi

@Strain 0.200 %
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.062 in (1.6 mm)
Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.062 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu..