Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.01 MPa | 581 psi | 200%, post cured- 8 hours at 200°C; ASTM D412 |
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |