Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.00 MPa | 580 psi | at 200%, no post cure- press cured for 5 minutes; ASTM D412 |
Multibase SILASTIC® 7-4860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 0350 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D412 |
Polymax® Maxelast® P1870 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 4.00 - 10.8 MPa | 580 - 1570 psi | Average value: 7.34 MPa Grade Count:21 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Yield | 4.00 - 369 MPa | 580 - 53500 psi | Average value: 32.1 MPa Grade Count:775 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | Support Rubber |
Fujipoly Industries Zebra® Silver Connector Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive laye.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ISO 527 |
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 50 mm/min; ISO 527-1/-2 |
Styrolution Styroflex® 2G 66 SBC Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3501-55-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3210-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg B500 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg B700 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Commercial Neoprene® C798 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg R608 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Z800 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Z900 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg B600 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 4.00 MPa @Strain 50.0 % |
580 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Nakan® FMM 611 N PVC, Soft Injection Molding Grade NAKAN FMM 611 N is a soft polyvinyl chloride compound developed for injection molding of breathing masks and general purpose.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | Film Property, 50 µm thickness; ASTM D882 |
Arkema Group OREVAC® 9304 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
ACC MM239 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: ceramic/polyester/PU/epoxy a.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
BASF Lucalen® A 2710 H Ethylene/Acrylate Copolymer Product with properties which are typical of flexible PVC and of low density polyethylene. Suitable for flexible pipes, profiles and seals.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 4.00 - 8.00 MPa | 580 - 1160 psi | Average value: 5.67 MPa Grade Count:3 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Z600 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ISO 527 |
Breplast Bretene SP Polypropylene / Polyethylene Composite Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |