Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 399 MPa @Strain 0.200 % |
57900 psi @Strain 0.200 % |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 399 MPa @Strain 0.200 % |
57900 psi @Strain 0.200 % |
|
Haynes Multimet® alloy, investment-cast, as-cast Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Yield | 399 MPa @Strain 0.200 % |
57900 psi @Strain 0.200 % |
|
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.250 in (6.4 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.250 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |