Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.41 MPa
5716 psi
ASTM D-638
Axiall 8266 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 39.41 MPa
5716 psi
ASTM D-638
Axiall 8266 Rigid PVC, Extrusion, Natural
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 39.41 MPa
5716 psi
ASTM D-638
Axiall 8266 Rigid PVC, Extrusion, White
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Copyright © lookpolymers.com All Rights Reserved