Polymer Property : Tensile Strength, Yield = 5475 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.75 MPa

@Temperature 23.0 °C
5475 psi

@Temperature 73.4 °F
ASTM D638
Ineos H38G-02 Polypropylene Homopolymer
This is a polypropylene homopolymer for general purpose injection molding and high speed spinning applications. It is useful for spun bonded nonwovens and partially oriented yarn (POY). This mater..