Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 375 MPa @Strain 0.200 % |
54400 psi @Strain 0.200 % |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Yield | 375 MPa @Strain 0.200 % |
54400 psi @Strain 0.200 % |
|
Haynes 556® alloy, 0% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 375 MPa @Strain 0.200 % |
54400 psi @Strain 0.200 % |
|
Haynes 556® alloy, bar, after 8000 hours at 760°C (1400°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 375 MPa @Strain 0.200 % |
54400 psi @Strain 0.200 % |
|
Haynes 556® alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 375 MPa @Strain 0.200 %, Temperature 95.0 °C |
54400 psi @Strain 0.200 %, Temperature 203 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Yield | 375 MPa @Strain 0.200 % |
54400 psi @Strain 0.200 % |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Yield | 375 MPa @Strain 0.200 % |
54400 psi @Strain 0.200 % |
Solution Annealed. Value at room temperature |
Special Metals INCONEL® Alloy HX A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high.. |