Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Oxford Polymers INJ-FR Glass Fiber Reinforced ABS, Flame Retardant Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | ASTM D638 |
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene Moplen HP562S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562S is a homopolymer particularly suitable f.. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | ASTM D638 |
PolyMirae Moplen HP562T Fiber (Spunbond) Grade Polypropylene Moplen HP562T is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562T is a homopolymer particularly suitable f.. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | ASTM D638 |
PolyMirae Moplen HP640R Injection Molding Grade Polypropylene Moplen HP640R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640R is a homopolymer particularly suitable for injection molding.. |
|||
Tensile Strength, Yield | 37.2 - 97.9 MPa | 5400 - 14200 psi | Average value: 71.3 MPa Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Tensile Strength, Yield | 37.3 MPa @Thickness 3.20 mm |
5400 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HI100 ABS, High Impact Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Ineos H44N-00 Polypropylene Homopolymer H44N-00 is a high flow rate, nucleated polypropylene homopolymer designed for compounding and injection molding applications. The grade benefits from a high stiffness and isotropic shrinkage to help.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Plastiblend® ABS E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VC-0830 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0812 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnum™ 2630 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnum™ 275 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnum™ 8325 ABS, Sheet Coextrusion Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnumâ„¢ FG960 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
PlastxWorld CEVIAN® E80 ABS Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 37.23 MPa | 5400 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 5101M Staple Fiber and Injection Molding Polypropylene HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101M is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA T-105 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP30-1200S Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Clariant Renol PP1112AS10 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | |
Atom Adhesives AA-BOND FS227 Epoxy Adhesive AA-BOND FS227 is a thixotropic polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, a.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Aaron Industries AVPP HOMO 200-1 Virgin Polypropylene A virgin polypropylene specifically designed for all injection molding applications. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Amco Amalloy® B1044 Polymer Alloy Amco Amalloy B1044 is a proprietary copolymer with exceptional clarity and toughness.Low haze, low melt flow, high tensile & flexural strength.Information provided by Amco Plastic Materials. |
|||
Tensile Strength, Yield | 37.3 MPa @Thickness 3.20 mm |
5400 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Spartech Royalite R12 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 25% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D-638 |
Axiall SP-6235 Rigid PVC, Molding Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall.. |