Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 360 - 480 MPa | 52200 - 69600 psi | Proof Stress |
Kennametal Stellite Denertiaâ„¢ N19 Nickel Dental Alloy Denertiaâ„¢ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium freeInformation provided by Kennametal St.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 %, Temperature 870 °C |
52200 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 25 alloy, cold worked sheet, 15 % cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 % |
52200 psi @Strain 0.200 % |
|
Haynes 556® alloy, bar, after 1000 hours at 870°C (1600°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 % |
52200 psi @Strain 0.200 % |
|
Haynes 625 alloy, 40% cold reduction, 1175°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | >= 360 MPa @Strain 0.200 % |
>= 52200 psi @Strain 0.200 % |
|
CLAL-MSX CUPROROR® TL4 Hard, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Tensile Strength, Yield | 360 - 400 MPa | 52200 - 58000 psi | T direction |
ArcelorMittal Torque 20-15 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 360 - 400 MPa | 52200 - 58000 psi | T direction |
ArcelorMittal Torque 25-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 360 - 400 MPa | 52200 - 58000 psi | T direction |
ArcelorMittal Torque 27-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 360 - 400 MPa | 52200 - 58000 psi | T direction |
ArcelorMittal Torque 30-17 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 360 - 400 MPa | 52200 - 58000 psi | T direction |
ArcelorMittal Torque 30-18 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 % |
52200 psi @Strain 0.200 % |
|
AK Steel 444 Ferritic Stainless steel AK Steel 444 is a low-carbon, low nitrogen, ferritic stainless steel that provides pitting and crevice corrosion resistance superior to most ferritic stainless steels. Applications requiring superi.. |
|||
Tensile Strength, Yield | 360 - 440 MPa | 52200 - 63800 psi | |
ArcelorMittal Complex Phase Steel 600 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT600C) and electrogalvanized (HCT600C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r.. |
|||
Tensile Strength, Yield | 360 - 435 MPa | 52200 - 63100 psi | |
ArcelorMittal HSLA 360 High strength low alloy steel for cold forming, Hot Rolled Available in the following: S355MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 % |
52200 psi @Strain 0.200 % |
|
Haynes 625 alloy, 10% cold reduction, 1175°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |