Tensile Strength, Yield 33.5 MPa

@Temperature 23.0 °C
4860 psi

@Temperature 73.4 °F
ASTM D638
Ineos H03G-04 Polypropylene Homopolymer
This is a polypropylene homopolymer for biaxially oriented polypropylene (BOPP) film and blow molding applications. This material meets the requirements of the U.S. Food and Drug Administration as ..
Tensile Strength, Yield 33.5 MPa
4860 psi
ISO 527-2
Borealis HB600TF Polypropylene
HB600TF is a low melt flow rate polypropylene homopolymer intended for extrusion and thermoforming. Its very good organoleptic properties allows this grade to be used with any master batch without ..
Tensile Strength, Yield 33.5 MPa
4860 psi
50mm/min; ISO 527-2
Borealis HD120MO Polypropylene
HD120MO is a polypropylene homopolymer with a good combination of mechanical properties intended for injection molding. Applications: sanitary equipment, caps and closures, and general packagingInf..
Tensile Strength, Yield 33.5 MPa
4860 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Zinc Stearate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tensile Strength, Yield 33.5 MPa
4860 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Zinc Stearate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..