Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 330 MPa | >= 47900 psi | |
MetalTek Nitronic® 40 Austenitic Stainless Steel Produced under license of ARMCO Advanced Materials Corp. Information provided by MetalTek |
|||
Tensile Strength, Yield | 330 MPa | 47900 psi | |
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Stainless steel 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Yield | 330 MPa @Strain 0.200 %, Temperature 540 °C |
47900 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 330 MPa @Strain 0.200 %, Temperature 650 °C |
47900 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 330 MPa @Strain 0.200 %, Temperature 205 °C |
47900 psi @Strain 0.200 %, Temperature 401 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Yield | 330 MPa @Strain 0.200 % |
47900 psi @Strain 0.200 % |
Annealed prior to test |
Special Metals BRIGHTRAY® Alloy C Electrical Resistance Alloy A nickel-chromium electrical-resistance alloy for use at operating temperatures up to 2100°F (1150°C). It contains rare-earth additions for increased oxidation resistance, especially under co.. |
|||
Tensile Strength, Yield | 330 MPa @Strain 0.200 %, Temperature 550 °C |
47900 psi @Strain 0.200 %, Temperature 1020 °F |
Solution Annealed prior to test |
Special Metals INCONEL® Alloy 601 A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temper.. |
|||
Tensile Strength, Yield | 330 MPa | 47900 psi | |
SSAB Tunnplat Domex® 014 BOR Rolled Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Yield | 330 - 410 MPa | 47900 - 59500 psi | |
ArcelorMittal Dual Phase 600 Very high strength steel, Cold Rolled Steel Available in the following: HCT780X (uncoated), HCT780X+ZE (electrogalvanized) and HCT780X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a.. |
|||
Tensile Strength, Yield | 330 - 460 MPa | 47900 - 66700 psi | |
ArcelorMittal Dual Phase 600 Very high strength steel, Hot Rolled Steel Available in the following: HCT580X (uncoated)Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martens.. |