Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
SABIC PP 49MK40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK40 is a high crystalline impact copolymer with high stiffness. This grade is especially developed for producing injection molded articles. The grade contains an antist.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Polymer Industries Densetec PP Homopolymer Sheet Polymer Industries’ Densetec Homopolymer Polypropylene exhibits the properties of high corrosion resistance, high temperature resistance, and great tensile strength. It maintains its stiffness at e.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | 50 mm/min |
Polimeri Europa KOBLEND HI 10 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend with very good impact behaviour, ductility even at low temperatures, resistant to solvents. Main application fields: autom.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ISO 527-2 |
Polyplastic Armlen® PP MF 25-3-901 Polypropylene, 20% Mineral Filled Heat stabilized, black colorInformation provided by PolyPlastic Group. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | 50 mm/min test speed; ASTM D 638 |
NOVA Chemicals Sclair® IG464-C Compression Molded HDPE Resin IG464-C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG464.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ISO 527-1, -2 |
LyondellBasell Moplen HP550J Polypropylene Homopolymer Description: HP550J, a general purpose polypropylene homopolymer resin, is suitable for general extrusion and film fiber applications. HP550J resin meets FDA requirements in the Code of Federal Reg.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Flint Hills P5M4K-046 Random Copolymer Polypropylene Random copolymer, FDA compliant.Features: Clarified (50 mil plaque haze 10%), antistat, and controlled rheology.Applications: Injection molding: high clarity parts, medical parts, and good organolep.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ISO 527-1, -2 |
LyondellBasell Hostacomâ„¢ CB267 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB267 medium melt flow, 1,600 MPa flexural modulus thermoplastic elastomeric olefin (TEO) resin has an excellent balance of scratch and mar resistance, rigidity and impac.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ISO 527-1, -2 |
LyondellBasell Hostacomâ„¢ TKS709D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TKS709D medium high melt flow, 1,600 MPa flexural modulus, UV-stabilized, thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and proc.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DZL34E PC (Asia Pacific) LNP* Lubricomp* DZL34E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP MG004 PP (Europe-Africa-Middle East) LNP* Lubricomp* MG004 is a compound based on Polypropylene resin containing Graphite Powder. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Total PPH 3727W Polypropylene, High Performance Injection Molding Grade Balanced Properties TOTAL Polypropylene 3727W strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Total PSI 3441 High Heat Resistance Impact Polystyrene Total Petrochemicals Polystyrene 3441 is a high heat resistance, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional st.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | GB/1040 |
Zhejiang Juner PP8 PP For Automotive Parts Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | 79% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Toluene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ISO 527-2/50 |
ExxonMobil PP1013H1 Polypropylene Homopolymer Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ISO 527-2/1A/50 |
ExxonMobil PP1304E3 Polypropylene Copolymer Product Description: A homopolymer resin designed for injection molding applications requiring excellent flow and good mechanical properties. It is designed for caps and closures, general applicati.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Entec Hypro™ PPH-T30 Homopolymer Polypropylene, 30% Talc Reinforced Information provided by Entec |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334C10L Calcium Reinforced |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334M30L Mica Reinforced |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334T30L Talc Reinforced |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336M20L Mica Reinforced |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336T40L1 Talc Reinforced |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM-D638 |
Braskem PRA 0852 RACO Random Polypropylene Copolymer PRA 0852 is a medium melt flow rate random copolymer with slip and antiblocking agents. It is suitable for blown and cast film extrusion. PRA 0852 has excellent optical properties and good processab.. |
|||
Tensile Strength, Yield | 33.0 MPa | 4790 psi | ISO R 527 |
Addiplast Addilene H 520 M40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 33.0 MPa @Temperature 80.0 °C |
4790 psi @Temperature 176 °F |
ISO Data |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |