Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 314 MPa | 45500 psi | |
Kennametal Stellite Stellite® 250 Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.Applications:heat treatment furnace.. |
|||
Tensile Strength, Yield | 314 MPa @Strain 0.200 % |
45500 psi @Strain 0.200 % |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Yield | 314 MPa @Strain 0.200 % |
45500 psi @Strain 0.200 % |
|
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |