Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o.. |
|||
Tensile Strength, Yield | >= 29.0 MPa | >= 4210 psi | ASTM D638 |
NIZHNEKAMSKNEFTEKHIM PP 4310M (EP1X30F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | |
Radici Radilon® CS 38FL (cond.) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 500 mm/min |
NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin Features: Excellent processability for applications requiring good stiffness and toughness, good cold temperature impact properties.Applications: Food containers and lids, frozen food containers.Dat.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
NOVA Chemicals Sclair® 2907 HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness, good top loading capability, high surface gloss.Applications: Protective sports equipment, safety helmets, high impact custom molding.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness.Applications: Tote boxes, beverage crates.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50 mm/min; ASTM D638 |
NOVA Chemicals Sclair® 2908C HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughnessApplications: Tote boxes, Beverage cratesAdditives: AntioxidantInformation provided by NOVA Chemicals. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
NOVA Chemicals Sclair® 59A HDPE Injection Molding Resin Features: Homopolymer, high drop impact resistance and high stiffness.Applications: Juice, water containers, personal protective equipment, grain elevator buckets, designed for accumulator and recip.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Global N-3260 High Density Polyethylene, Yarn/Monofilament Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing nets, wire & cable insulators, auto parts, pipesInformation provided by Global .. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Flint Hills 23S1Acs256 Random Copolymer Polypropylene Features: High contact clarity, blush resistant, good impact and flexural modulus. Product does not contain animal derived components.Applications: Blow molded articles - Food, health, medical an.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Flint Hills P9H8M-058X Specialty Polypropylene Features: Does not contain animal derived components. Product is Phthalate-free. A low phosphorus content material.Applications: Extrusion coating. Suitable for silicone coating.Information pro.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450EX PBT (Asia Pacific) LNP* Thermocomp* WH0450EX is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50mm/min; ISO 527-2 |
Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA415E is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength. This material has been designed for improved processability and.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50mm/min; ISO 527-2 |
Borealis RF926MO Polypropylene, Transparent Random Copolymer RF926MO is a specially modified transparent polypropylene random copolymer with high melt flow. This grade is intended for injection stretch blow molding (ISBM). and is designed for high-speed injec.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ISO 527-2 |
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene DescriptionPolyfort® FPP 1237 is a 20% CAC03 filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 2 in/min, Type IV bar; ASTM D638 |
Chevron Phillips Marlex® K605 HDPE Blow Molding Resin Resin Type: Ethylene HomopolymerCharacteristics: Good ESCRExceptional rigidityExcellent melt strengthApplications: Automotive bumper beamsInformation provided by Chevron Phillips. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Entec Hypel® PEHD18/.956 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high .. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50 mm/min; ISO 527 |
Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336C30L1 Calcium Reinforced |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM-D638 |
Braskem Prisma 3410 RACO Random Polypropylene Copolymer Prisma 3410 is a medium melt flow rate random copolymer designed for injection molding. This product exhibits exceptional transparency, very good stiffness/impact strength balance, and excellent pro.. |
|||
Tensile Strength, Yield | 29.0 - 186 MPa | 4210 - 27000 psi | Average value: 68.8 MPa Grade Count:40 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 2.0 in/min; ASTM D638 |
Ineos Nova Zyntar® 351 High Performance Flame Retardant Polystyrene
(discontinued **) High Vicat and heat reflection temperature, Custom colorsApplications: Injection molding, Gas-assist injection molding, Structural foam, TV cabinets, Electronic enclosuresThis is an impact grade of .. |