Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials FCC-221-P Copper Steel Powdered Metal Applications:Medium strength mechanical componentsEquivalent MPIF Specification: FC-0205-35All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials FN-251-S Invar Powdered Metal Coefficient of thermal expansion equal to glass.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials SS-316-RD 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Equivalent MPIF Specification: SS-316-40All information provided by Pacific Sin.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RD Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance. Equivalent MPIF Specification: SS-316-40Information Provided by Pacific Sinte.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
PSM Industries Pacific Sintered Metals High Carbon Steel F-244-S Powdered Metal Highly stressed mechanical components, Good hardenability Equivalent MPIF Specification: F-0008-35Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Kinetics MIM F15 (Kovarâ„¢) Low CTE Alloy High nickel, high cobalt iron alloy. A traditional metal-to- glass sealing alloy that offers a low coefficient of thermal expansion (CTE) similar to glass. Provides the hermeticity required for firm.. |
|||
Tensile Strength, Yield | 276 - 345 MPa @Strain 0.200 % |
40000 - 50000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | >= 276 MPa | >= 40000 psi | |
MetalTek MTEK WC 9 Cast UNS J42045 Alloy Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 %, Temperature 538 °C |
40000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 276 - 483 MPa | 40000 - 70100 psi | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 %, Temperature 538 °C |
40000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton RV00AESM PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESM is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Moldin, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
Heat Treated |
Universal Wire Works 410 Stainless Steel (AMS 5776) Filler Metal Universal 410 is a ferritic stainless steel alloy, primarily used as filler metal for gas metal arc and gas tungsten arc welding of steel of similar composition. Deposits are resistant to corrosion .. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
Universal Wire Works Inconel 62 (AMS 5679) Nickel Alloy Filler Metal Inconel Filler Metal 62 is a nickel chromium alloy designed for welding nickel base alloy 600 in up to 2" thicknesses using the gas tungsten arc, gas metal arc and submerged arc processes. Filler Me.. |
|||
Tensile Strength, Yield | >= 276 MPa | >= 40000 psi | Larger sizes may be lower. |
Alcoa Toolrite 2011®-T8 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Tensile Strength, Yield | 276 - 345 MPa | 40000 - 50000 psi | 0.2% offset |
Eagle Brass 151 ZHC® COPPER, 1/2 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Yield | 276 - 379 MPa | 40000 - 55000 psi | 0.2% offset |
Eagle Brass 519 Phosphor Bronzes 6%, 1/4 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
Crucible Steel 347 Chromium-Nickel Steel Crucible 347 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | Premium Casting |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Yield | >= 276 MPa @Strain 0.200 % |
>= 40000 psi @Strain 0.200 % |
|
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | Annealed |
California Fine Wire Alloy 52 Nickel Iron Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 %, Temperature 93.0 °C |
40000 psi @Strain 0.200 %, Temperature 199 °F |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
Carpenter 20-Mo6® Stainless Steel, Strip Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® 330 UNS N08330 Nickel Superalloy Uses: Weld wire, woven wire mesh belts, rod for heat treat baskets, heat treat fixtures.Property values are for samples in the metallurgical condition: As rolled.Information provided by Allvac, An A.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® Grade 7 UNS R52400 Titanium Alloy Uses: Industrial components, CPI equipment, heat exchangers, pressure vessels, fittings, tubings.Property values are for samples in the metallurgical condition: 1300°F anneal.Information provided b.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal Data provided by Allvac.Applications: Afterburner components, combustion chamber liners, nozzles, vanes, rings, turbine exhaust weldments, structural parts. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® 40, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | ISO 527-2 |
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Tensile Strength, Yield | >= 276 MPa | >= 40000 psi | Minimum |
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |