Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.5 MPa | 3990 psi | ASTM D683 |
Chevron Phillips Marlex® HMN 55180 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This resin is a narrow molecular weight distribution copolymer with easy processing characteristics and excellent toughness properties. This product disp.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | ASTM D638 |
Flint Hills 23M2A Polypropylene Random Copolymer Features: High contact clarity, blush resistant, good impact, and stress resistant, good auto-clave stability, and low extractability. Product does not contain animal derived components.Application.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | ASTM D638 |
Flint Hills AP5995-HA Polypropylene Impact Copolymer Features: Nucleated with slip, fast cycle times, high flowability.Applications: Injection Molding: High speed packaging applications and thin wall containersInformation Provided by Flint Hills Resou.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | ASTM D638 |
Ineos L10G-00 Polypropylene Impact Copolymer L10G-00 is a barefoot polypropylene impact copolymer designed for injection molding applications. It offers excellent impact resistance, high flexural modulus and good processability. This material .. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | ASTM D638 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | ASTM D638 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | 50 mm/min; ASTM D638 |
LG Chemical 501S-S HIPS Self lubricant, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food holders, par.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | 66% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | ASTM D638 |
Tipco Tipcolene® FPC 10 PPC - 10% Calcium Carbonate Reinforced Polypropylene Copolymer 10% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | ASTM D638 |
Tipco Tipcolene® FPC 30 - 30% Calcium Carbonate Reinforced Polypropylene Homopolymer 30% Calcium Carbonate Filled PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | 300% elongation |
Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3990 psi | 50 mm/min; ASTM D638 |
LG Chemical 402 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include t.. |