Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 272 MPa @Temperature 649 °C |
39500 psi @Temperature 1200 °F |
|
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |