Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ISO 527-2 |
Total Lacqrene® 4240(EU) High Impact Polystyrene
(discontinued **) LACQRENE® 4240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of good rigidi.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ISO 527-2 |
Total Lacqrene® 4241 High Impact Polystyrene
(discontinued **) DescriptionLACQRENE® 14240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
Braskem BS 002J HDPE Blow Molding Polyethylene
(discontinued **) Applications: Bottles up to 60 liters with high ESCR; bottles for surface-active agents. Information provided by Braskem |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638M |
DSM Somos® 8120 Epoxy Photopolymer
(discontinued **) DescriptionDSM Somos® 8120 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and .. |
|||
Tensile Strength, Yield | 26.0 - 62.0 MPa | 3770 - 8990 psi | Average value: 42.5 MPa Grade Count:4 |
Overview of materials for Nylon 6/69 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer INNOPOL® CS 3-9230 KAR YU is a yellow colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR YU is develop.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
IRPC Polimaxx Polene 3325M Polypropylene Random Copolymer CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD SEALABLE CONTAINS SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM EXTRUSION CPP FILM FOR LAMINATE , CPP FILM FOR PACKAGINGS |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
Flint Hills P5M4R-034 Polypropylene Random Copolymer Features: Radiation resistant. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: medical devicesInformation Provided by Flint Hills Resources |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON TD000 PU LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WX02869H Polyester, TP LNP THERMOCOMP* WX02869H is a compound based on Polyester, TP resin containing High Specific Gravity. Added features of this material include: High Impact. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | 50mm/min; ISO 527-2 |
Borealis BL0521 High Density Polyethylene BL0521 is a high molecular weight (HMW), high density polyethylene. The main properties are: good impact resistance, high stiffness, very good stress crack resistance. Applications: cans and drums .. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | 24 min.; ASTM D638 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | 50mm/min; ISO 527-2 |
Borealis MG9621B Polyethylene Applications: crates, and pailsInformation provided by Borealis AG |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ISO 527 |
Unipetrol PP MONSTEN® MT 825 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ISO 527 |
Unipetrol PP MONSTEN® MT 935 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | 24 min.; ASTM D638 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
Total PSI 8350 (AS) High Impact Polystyrene Total Petrochemicals Polystyrene 8350 (AS) is a very high impact polystyrene for extrusion and injection molding. This grade has improved environmental stress crack resistance in comparison with st.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | 2 in/min; ASTM D638 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ISO 527 |
Unipetrol PP MONSTEN® MT 805 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | Type 1 @ 2 in/min; ASTM D638 |
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | Type 1 @ 2 in/min; ASTM D638 |
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Fin.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | parallel; ISO 527-3 |
Covestro Desmopan® W DP 85786A Polyurethane Grade for calanderingno yellowing under the action of UV lightgood low-temperature flexibilityhigh rebound resilienceimproved microbial resistanceImproved hydrolysis resistanceApplicationTextile coa.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
Entec Hypro™ PPH-CC30 Natural Homopolymer Polypropylene, 30% Calcium Carbonate Filled Information provided by Entec |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
Aclo Accuguard Polypropylene CP0467V0CSL Copolymer Flame Retardant Copper Stabilized |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | 2 in/min (50 mm/min); ASTM D638 |
Bapolene® 3252 Polyethylene, Injection Grade Narrow molecular weight distribution injection molding resin. This resin offers excellent impact strength, ESCR properties, and resistance to warpage. This product meets the Food and Drug Administ.. |
|||
Tensile Strength, Yield | 26.0 MPa @Strain 50.0 % |
3770 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
Aclo Accutech Polypropylene CP0405UVV Copolymer UV Stabilized Approved to Suzuki PP-S2 Med Grey T01 |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ISO 527-2 |
Total PPC 3120 MU5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene PPC 3120 MU5 is a heterophasic copolymer with a Melt Flow index of 15 g/10 min. Polypropylene PPC 3120 MU5 is a high impact copolymer formulated to give good UV resistance.Polypropyle.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | 50 mm/min |
Arkema Group Kynar® FLEX 2800 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1N, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, impervious.. |
|||
Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
Ineos Nova 6100 Super High Impact Polystyrene
(discontinued **) Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen.. |