Tensile Strength, Yield 25.30 MPa
3669 psi
2"/min; ASTM D638
ICO Polymers ICORENEâ„¢ 150-1050 HDPE Rotational Molding Resin
Description: ICORENE 150-1050 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is..
Tensile Strength, Yield 25.30 MPa
3669 psi
2"/min; ASTM D638
ICO Polymers ICORENEâ„¢ 150-1497 HDPE Rotational Molding Resin
Description: ICORENE 150-1497 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. Applications: Th..
Tensile Strength, Yield 25.30 MPa
3669 psi
2"/min; ASTM D638
ICO Polymers ICORENEâ„¢ 150-1500 HDPE Rotational Molding Resin
Description: ICORENE 150-1500 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is ..
Tensile Strength, Yield 25.30 MPa
3669 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N990 (MT) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 25.30 MPa
3669 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N990 (MT) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..