Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.48 MPa | 360 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 653 Perfluoroelastomer Chemraz® is a black perfluoroelastomer specifically formulated to meet the extreme demands of diffusion, LPCVD and thin dry processing applications. It exhibits superior compression set resistan.. |
|||
Tensile Strength, Yield | 2.48 MPa | 360 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3311-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 2.48 MPa | 360 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-45 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 2.48 MPa | 360 psi | |
Master Bond Mastersil 150 Two Part, Condensation Cured, Flexible Silicone Master Sil 150 is a 2 part condensation cured liquid silicone which, after the addition of curing agent 150, cures at room temperature to a tough, resilient silicone rubber potting and encapsulation.. |
|||
Tensile Strength, Yield | 2.48 MPa | 360 psi | |
Master Bond Mastersil 801 One Component, Room Temperature Curing, Silicone System MasterSil 801 is an easy to use, one component, high performance silicone elastomer compound. MasterSil 801 features non-corrosive cure and serviceability up to 300°C; it exhibits good stability at.. |