Polymer Property : Tensile Strength, Yield = 3448 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.77 MPa
3448 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tensile Strength, Yield 23.77 MPa
3448 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..