Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-2002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 22.8 MPa @Thickness 3.20 mm |
3300 psi @Thickness 0.126 in |
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 2150 H Medium Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 22.8 MPa @Thickness 3.20 mm |
3300 psi @Thickness 0.126 in |
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 3220 Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® L63935 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering .. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | Type I, 2 in/min; ASTM D638 |
M. Holland Company CP502 Polypropylene Copolymer Features: Copolymer, High Flow, High Impact ResistanceUses: Closures, Medical Applications, Thin-walled PartsProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
Multibase Multi-Flamâ„¢ 0220 PP Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsUses:TubingWire JacketingFurnitureInformation provided by Multibase |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
Multibase Multi-Flamâ„¢ 0901 HDPE Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Blow MoldingExtrusionCoextrusionUses:TubingFurniturePipingInformation provided by Multibase |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
Spartech Litho SP-2090 Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-882 |
Saint-Gobain Norton® F710 Chemically Resistant Skived PTFE Sheet Description: PTFE = polytetrafluoroethyleneApplications include: Chemical Resistant; Common in Electrical/ElectronicsInformation provided by Saint Gobain Performance Products. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7100-50D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2"/min; ASTM D638 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2"/min; ASTM D638 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total CD 4300 HDPE extrusion Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product.. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
ExxonMobil HDPE HD 6601.29 High Density Polyethylene Copolymer Resin Product Description: HD 6601 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance... |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-638 |
Axiall 1901 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-638 |
Axiall 21540 Coax & Telecom Flexible PVC Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation.Information provided by Georgia GulfGeorgi.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
Asahi Kasei Thermofil P-40CC-1100 40% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total Finathene® 4344 HDPE, blow molding
(discontinued **) Applications: storage tank liners, intermediate bulk containers, general large-part blow molding. Blow Molding Stock Temperature 370 – 410 ºFInformation provided provided by Total Petrochemicals.T.. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-638 |
Axiall 8450 Moldings & Extrusions Flexible PVC High durometer, general purpose extrusion compound formulated for microbial resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total Finathene® CD 481 HDPE conduit
(discontinued **) Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-638 |
Axiall 4520 Flexible PVC Non-lead stabilized, thin wall, 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |