Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.6 MPa @Thickness 2.00 mm |
3270 psi @Thickness 0.0787 in |
50mm/min; ASTM D638 |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638 |
Global F-8000 High Density Polyethylene Description-good mechanical strengthApplications-blown wide film applications producing liner film & industrial filmInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638 |
Global MB-6366 High Density Polyethylene Description-high density for high quality, excellent creep & chemical resistanceApplications-drinking water pipe, industrial pipe, sewer pipeInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC T3410 Polypropylene Random Terpolymer Features: Seetec T3410 is a polypropylene-ethylene-butene random terpolymer designed for the production of Transparent Film and Expandable PP for low seal temperature and high impact strength. It of.. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 20 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 20 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 20 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 20 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ H511W High Density Polyethylene Wire & Cable Grade Key Characteristics: Contains special metal deactivator, high mechanical properties, high speed extrusionRecommended Applications: Insulation of communication cablesInformation provided by SCG Che.. |
|||
Tensile Strength, Yield | >= 22.5 MPa | >= 3270 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | >= 22.5 MPa | >= 3270 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | >= 22.5 MPa | >= 3270 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | >= 22.5 MPa | >= 3270 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | |
Zylog Hipolyene® 7151 M1 HF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | >= 22.5 MPa | >= 3270 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | |
Zylog Hipolyene® 1532 HC EX Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638 |
Total Lacqrene® 814(AS) High Impact Polystyrene
(discontinued **) LACQRENE® 814 is a high impact, flame retardant polystyrene, free from PBDPE and with excellent thermal stability.ApplicationCovers for electrical equipment, Office equipment: copiers, faxInformati.. |
|||
Tensile Strength, Yield | >= 22.5 MPa | >= 3270 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638M |
Total Lacqrene® 4431 Flame Retardant Polystyrene
(discontinued **) LACQRENE ® 4240 is a high impact, flame retardant polystyrene with excellent thermal stability.ApplicationTelevision back coversInformation provided provided by Total Petrochemicals.Total Petrochem.. |