Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 219 MPa | 31800 psi | ASTM D638 |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |