Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.0 MPa | 3040 psi | |
Spartech E65390 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3040 psi | ASTM D412 |
Teknor Apex APEX® 1700-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3040 psi | 2.0 in/min; ASTM D638 |
ExxonMobil PP143KNE1 Polypropylene Homopolymer Product Description: A high impact copolymer resin designed consumer and industrial applications.Availability: North America Features:Good ColorabilityGood Dimensional StabilityGood Mold ReleaseGoo.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3040 psi | 2.0 in/min; ASTM D638 |
ExxonMobil PP7505KNE2 Polypropylene Homopolymer Product Description: A medium to high impact copolymer designed for injection molded large consumer and industrial parts requiring high melt flow rate.Availability: North America Features:Balanced .. |
|||
Tensile Strength, Yield | 21.0 MPa | 3040 psi | 2.0 in/min; ASTM D638 |
ExxonMobil PP8255E1 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact copolymer resin designed for compounded and injection molded applications requiring high melt flow rate and excellent processing attributes... |