Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.08 MPa
302 psi
ASTM D412
Polymax® Maxelast® P2645 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield >= 2.08 MPa
>= 302 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5861 Fluoro-silicone
Fluoro-silicone meeting MIL-R-25988BInformation provided by Seals Eastern, Inc.