Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding 50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | |
Pacific Sintered Materials FN-255-S Nickel Steel Powdered Metal Good impact resistant mechanical components. Good hardenability.Equivalent MPIF Specification: FN-0205-25All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Solvay Specialty Polymers Kadel® E-1230 Polyketone
(discontinued **) Electrical Conductor. High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, p.. |
|||
Tensile Strength, Yield | 207 MPa @Strain 0.200 %, Temperature 871 °C |
30000 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF33 HS NAT 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Tensile Strength, Yield | 207 - 414 MPa @Strain 0.200 % |
30000 - 60000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann.. |
|||
Tensile Strength, Yield | 207 - 345 MPa @Strain 0.200 % |
30000 - 50000 psi @Strain 0.200 % |
Annealed temper |
Special Metals INCONEL® 601GC® Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 L BN047 LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: BeigeInformation.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® TPX-HTN-01027 A 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton RV008ESV PA 66 40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | >= 207 MPa | >= 30000 psi | 0.2% Offset |
Eagle Brass 302 Austenitic Stainless Steel, Annealed Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | >= 207 MPa | >= 30000 psi | 0.2% Offset |
Eagle Brass 316 Austenitic Stainless Steel, Annealed The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Tensile Strength, Yield | 207 MPa @Strain 0.200 % |
30000 psi @Strain 0.200 % |
|
Crucible Steel 316L Chromium-Nickel Steel Crucible 316L is a non-hardenable, low carbon austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Crucible 316L is designed for special applications requiring resi.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Clariant Renol PA111G50IF Nylon 66, 50% Glass Fiber, Improved Flow Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | |
CMW® ELKALOY D Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Tensile Strength, Yield | 207 - 303 MPa | 30000 - 44000 psi | 0.2% offset |
Eagle Brass 102 OF COPPER (Non-Certified), 1/2 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Yield | >= 207 MPa | >= 30000 psi | 0.2% Offset |
Eagle Brass 304 Austenitic Stainless Steel, Annealed Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | 207 MPa @Strain 0.200 % |
30000 psi @Strain 0.200 % |
|
Crucible Steel 304L Chromium-Nickel Steel Crucible 304L is a non-hardenable, low carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it i.. |
|||
Tensile Strength, Yield | >= 207 MPa @Strain 0.200 % |
>= 30000 psi @Strain 0.200 % |
|
Carlson C 800 Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | Typical |
Alpase M-1™ Aluminum Mold Plate M-1™ features and benefits include: Dimensional stability, fully weldable, anodizable, consistent hardness - regardless of size, can be nickel plated, good machinability, no heat treatment required.. |
|||
Tensile Strength, Yield | 207 MPa @Strain 0.200 % |
30000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® 601 UNS N06601 Nickel Superalloy Uses: Weld wire, woven wire mesh belts, rod for heat treat baskets, heat treat fixtures.Property values are for samples in the metallurgical condition: 1950°C anneal.Information provided by Allvac,.. |
|||
Tensile Strength, Yield | 207 MPa @Strain 0.200 %, Temperature 371 °C |
30000 psi @Strain 0.200 %, Temperature 700 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Tensile Strength, Yield | 207 MPa @Temperature 427 °C |
30000 psi @Temperature 801 °F |
Annealed |
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high du.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific) LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AM-40CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |