Tensile Strength, Yield 20.2 MPa
2930 psi
ASTM D412
Polymax® Maxelast® P3892 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 20.2 MPa
2930 psi
ASTM D638
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene
MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b..
Tensile Strength, Yield 20.2 MPa
2930 psi
Type IV specimen, 2" per minute test speed, 0.075" thickness compression molded samples; ASTM D 638
NOVA Chemicals Surpass® RMs341-U Octene sHDPE Rotational Molding Resin
RMs341-U complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341-..
Tensile Strength, Yield 20.2 MPa
2930 psi
Type IV specimen, 2" per minute test speed, 0.075" thickness compression molded samples; ASTM D 638
NOVA Chemicals Surpass® RMs341-UG Octene sHDPE Rotational Molding Resin
RMs341-UG complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341..
Tensile Strength, Yield 20.2 MPa
2930 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
LyondellBasell DEXFLEX® 940 TPO
Description: DEXFLEX® 940 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior painted applications. Applications: Bumper fascias, claddings Information provided by ..
Tensile Strength, Yield 20.2 MPa
2930 psi
ASTM D412
Elastocon TPE Technologies Elastocon® SMR1600 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1600 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..