Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.00 MPa | 290 psi | Conductive Layer |
Fujipoly Industries Zebra® Silver Connector Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive laye.. |
|||
Tensile Strength, Yield | >= 2.00 MPa | >= 290 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7075 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.00 MPa | 290 psi | ISO 527 |
Styrolution Styrolux S SBC Styrolux S is a new developmental, clear styrene-butadiene copolymer (SBC) designed specifically for blending with Styrolux T in order to enable high performance film extrusion and shrink film appli.. |
|||
Tensile Strength, Yield | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
|
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries. |
|||
Tensile Strength, Yield | 2.00 MPa | 290 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8400 Polyolefin Elastomer Description: Engage® 8400 and Engage® 8407 polyolefin elastomers are ethylene-octene copolymers that offer excellent performance in durable injection molded industrial and consumer goods and compr.. |
|||
Tensile Strength, Yield | 2.00 MPa | 290 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8407 Polyolefin Elastomer Description: Engage® 8407 polyolefin elastomer is an ethyleneoctene copolymer with a nominal loose talc coating. The talc is untreated and has a 1µm particle size. Engage® 8407 offers excellent p.. |
|||
Tensile Strength, Yield | 2.00 MPa | 290 psi | |
ACC MM906 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tensile Strength, Yield | 2.00 MPa | 290 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 36-018 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerGood Surface AppearanceOpaqueApplications:AutomotiveInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by P.. |
|||
Tensile Strength, Yield | 2.00 MPa | 290 psi | ASTM D3574 |
Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |
|||
Tensile Strength, Yield | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® ST-6350 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |