Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 196 MPa @Thickness 3.20 mm |
28400 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID SG2460B PA66+GF46%, General purpose, Good Surface Feature: Injection Molding, PA66+GF46%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base PlateCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 196 MPa | 28400 psi | 5 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Tensile Strength, Yield | >= 196 MPa | >= 28400 psi | |
Saint-Gobain Norslide® EKO-B PTFE Sliding Tubing Features/Benefits:Low stick-slip effectMaintenance free, no lubrication requiredWeatherproofIsolates noise, dampens vibrationFlexible and resilientResistant against fuel, oil, and greasesService tem.. |
|||
Tensile Strength, Yield | 196 MPa | 28400 psi | ASTM D638 |
Cheng Yu Plastic NG1400S Nylon 66, 40% Glass Fiber Reinforced |
|||
Tensile Strength, Yield | 196 MPa | 28400 psi | Dry; ASTM D638 |
Asahi Kasei Leona® 13G43 43% Glass Filled Nylon 66 43% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Mechanical and electrical parts such as micromotors, automotive parts such as radiator tanks and shift leversInformation provi.. |
|||
Tensile Strength, Yield | 196 MPa | 28400 psi | Wet; ASTM D638 |
Asahi Kasei Leona® 90G50 50% Glass Filled Nylon 66 Enhanced strength and stiffness; with 50% GF. Excellent appearance.Applications:Office furnitureInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 196 MPa | 28400 psi | ISO 527-2/1A/5 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |