Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 19.3 MPa | 2800 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 1802-xx05FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JC156HN Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx93FRSD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
Resinlab® CYNERGY CA6101 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
Resinlab® CYNERGY CA6103 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
Resinlab® CYNERGY CA6205 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 8 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
Resinlab® CYNERGY CA6102 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
Resinlab® CYNERGY CA6203 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
Resinlab® CYNERGY CA6204 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
Resinlab® CYNERGY CA6207 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
Resinlab® CYNERGY CA6208 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Tensile Strength, Yield | >= 19.3 MPa | >= 2800 psi | ASTM D1708 |
Technetics Group Texolon™ 7865 PTFE
(Unverified Data**) Virgin PTFE for those applications not requiring the premium qualities of 8764 sheet.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surfac.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D638 |
LyondellBasell Petrothene® KR92828 High Density Polyethylene ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | 2 in/min; ASTM D638 |
Ineos K38-20-188 HDPE K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural .. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D412 |
Teknor Apex APEX® 3300-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D412 |
Teknor Apex APEX® 90-P513A-80-NT Polyvinyl Chloride+PUR Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | At 50 mm/min; ASTM D683 IV |
Borealis Borecene Compact™ RM8346 Black Linear Polyethylene for Rotational Molding Borecene Compact RM8346 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides .. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D638 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D638 |
Westlake Plastics HIPS High Impact Polystyrene, Compression Molded Compression molded HIPS is a low cost plastic material that is easily machined and fabricated. It is frequently used for preproduction prototyping. HIPS is a FDA compliant use in food processing a.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D638 |
Total PSI 945 Polystyrene Polystyrene 945 is designed for injection molding applications requiring superior toughness. This polymer is a high impact polystyrene with excellent gloss and falling dart properties. The impact an.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D638 |
Westlake Plastics HIPS High Impact Polystyrene HIPS is a low cost plastic material that is easy to machine and fabricate. It is often specified for low strength structural applications when impact resistance, machinability, and low cost are req.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | Type IV; 50 mm per min; ASTM D638 |
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D638 |
ExxonMobil Paxon™ 7003 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | 50 mm/min cross speed; ASTM D638 |
DuPont™ Surlyn® 7930 Ionomer Resin, Lithium Surlyn® 7930 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D-638 |
Axiall 14880 Wire & Cable Flexible PVC 14880 is a non-lead stabilized, 80°C rated jacket with UL recognition for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D-638 |
Axiall 19890 Wire & Cable Flexible PVC Highly recommended for 105°C, 15 mil wall insulations and jackets where good gasoline and oil resistance is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
Tensile Strength, Yield | 19.3 MPa | 2800 psi | ASTM D-638 |
Axiall 38511 Wire & Cable Flexible PVC Tray cable jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 19.3 - 45.0 MPa | 2800 - 6530 psi | Average value: 34.2 MPa Grade Count:35 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |