Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Oxford Polymers Oxnilon 66-43GF 43% Glass Fiber Filled Nylon 66 for Injection Molding 43% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF HS UV 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcements, 33% Filler by WeightAdditive: Lubricant, Heat Stabilizer and UV Stabilizer Features: Lubricated, Good UV Re.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: LubricatedTPCI# 8682101Information provided by TP Composite.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 L UV 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceTPCI# 82.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 LE 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Extraction ResistantProcessing Method: Injection MoldingInformation provided b.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PET GF45 X 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Asahi Kasei Thermylon® NSG-440A-H 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |