Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6906 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excel.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized. Available as natural and several colors powder compounds.High quality Polyethylene re.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6006 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6007 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6013 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6015 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6303 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6309 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6809 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6813 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6902 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® L63568 Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568 is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® L63568U Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. Th.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D638 |
Ineos B35-150-134 MDPE
(discontinued **) Fortiflex® B35-150-134 is an intermediate density polyethylene copolymer developed for injection blow molding. It exhibits excellent gloss and environmental stress crack resistance (ESCR) in molde.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6001 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6004 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6801 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6803 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6810 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D638 |
Techmer ES HiFill® PP 0159 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SFE 3500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SMG 3500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Zylog Hipolyene® 5198 FLM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D-638 |
Axiall 10840 Wire & Cable Flexible PVC High gloss jacket and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D412 |
Teknor Apex APEX® 3201-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D638 |
ExxonMobil Escorene® HD-8660 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D638 |
ExxonMobil Escorene® HD-8660 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8660 is fully formula.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6905 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6908 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |