Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.00 MPa | 2611 psi | At 50 mm/min; ISO 527-3 |
Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.Borcoat HE0433 is primarily designed to be used as the tie laye.. |
|||
Tensile Strength, Yield | 18.00 MPa | 2611 psi | At 50 mm/min; ISO 527-2 |
Borealis BorPEX™ HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)) BorPEX HE2590 is a high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for electron beam irradiation crosslinking. The stabilization is optimized .. |
|||
Tensile Strength, Yield | 18.00 MPa | 2611 psi | At 50 mm/min; ISO 527-2 |
Borealis BorPEX™ HE2595 Black High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)) BorPEX HE2595 is a black, molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for electron beam irradiation crosslinking. The stabilization package is .. |