Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 17.9 MPa | 2590 psi | |
Spartech 2850-80 PVC for Regulated Applications Information provided by Spartech |
|||
Tensile Strength, Yield | 17.9 MPa | 2590 psi | |
Spartech E65080 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |