Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1.75 MPa | >= 254 psi | ASTM D412 |
Precision Polymer Engineering S70S Conductive Silicone Rubber Tan coloured, Silicone Rubber, 71-80 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber.Applications: Specially compounded to offer excellent physical and electrical properties.. |