Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.48 MPa
2535 psi
-8% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G80T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter..
Tensile Strength, Yield 17.48 MPa
2535 psi
ASTM D-638
Axiall 1063-119i Coax & Telecom Flexible PVC
Highly flame retardant CMR jacket for use over HDPE inners in 20-22 mil wall applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.